This post defines submerged arc welding process and includes a very instructive video that explains the process in detail.
Anodic polarization curves UNS N07718 (140K) in 3.5% NaCl
This post illustrates three cyclic anodic polarization curves of the precipitation hardening nickel alloy (PHNA) UNS N07718 —with a Specified Minimum Yield Strength of 140 ksi— in 3.5 wt% NaCl (pH 8.0).
Anodic polarization curves UNS N07718 (120K) in 3.5% NaCl
This post illustrates three cyclic anodic polarization curves of the precipitation hardening nickel alloy (PHNA) UNS N07718 —with a Specified Minimum Yield Strength of 120 ksi— in 3.5 wt% NaCl (pH 8.0).
Anodic polarization curves UNS N07718 (mill annealed) in 3.5% NaCl
This post illustrates three cyclic anodic polarization curves of the precipitation hardening nickel alloy (PHNA) UNS N07718 —mill annealed— in 3.5 wt% NaCl (pH 8.0).
Unusual Correlation between SKPFM and Corrosion of Nickel Aluminum Bronzes – Publication
In this article, we investigate the inverse correlation between Volta potentials measured by SKPFM and the observed localized corrosion morphology of NAB.
Materials and corrosion trends in offshore and subsea oil and gas production – Publication
In this article, we discuss materials and corrosion research topics that could have a transformative effect on the business. In particular, we discuss how scientists and engineers could push the boundaries of existing technologies, learning from the experience gained by other industries such as the nuclear, aerospace, and defense sectors.